Direct comparison of the bond strength results of the different test methods: a critical literature review SS Scherrer, PF Cesar, MV Swain Dental materials 26 (2), e78-e93, 2010 | 750 | 2010 |
The fracture resistance of all-ceramic crowns on supporting structures with different elastic moduli. SS Scherrer, WG De Rijk International Journal of Prosthodontics 6 (5), 1993 | 363 | 1993 |
Stimulating effect of implant loading on surrounding bone: Comparison of three numerical models and validation by in vivo data A Mellal, HWA Wiskott, J Botsis, SS Scherrer, UC Belser Clinical oral implants research 15 (2), 239-248, 2004 | 345 | 2004 |
Low temperature degradation of a Y-TZP dental ceramic M Cattani-Lorente, SS Scherrer, P Ammann, M Jobin, HWA Wiskott Acta biomaterialia 7 (2), 858-865, 2011 | 309 | 2011 |
Clinical outcome of three-unit lithium-disilicate glass–ceramic fixed dental prostheses: up to 8 years results S Wolfart, S Eschbach, S Scherrer, M Kern Dental materials 25 (9), e63-e71, 2009 | 246 | 2009 |
Fractographic analyses of three ceramic whole crown restoration failures JB Quinn, GD Quinn, JR Kelly, SS Scherrer Dental Materials 21 (10), 920-929, 2005 | 238 | 2005 |
Fracture rates and lifetime estimations of CAD/CAM all-ceramic restorations R Belli, A Petschelt, B Hofner, J Hajtó, SS Scherrer, U Lohbauer Journal of dental research 95 (1), 67-73, 2016 | 202 | 2016 |
Effect of cement film thickness on the fracture resistance of a machinable glass-ceramic SS Scherrer, WG De Rijk, UC Belser, JM Meyer Dental Materials 10 (3), 172-177, 1994 | 197 | 1994 |
Comparison of three fracture toughness testing techniques using a dental glass and a dental ceramic SS Scherrer, IL Denry, HWA Wiskott Dental materials 14 (4), 246-255, 1998 | 193 | 1998 |
Fatigue behavior in water of Y-TZP zirconia ceramics after abrasion with 30 μm silica-coated alumina particles SS Scherrer, M Cattani-Lorente, E Vittecoq, F de Mestral, JA Griggs, ... Dental materials 27 (2), e28-e42, 2011 | 189 | 2011 |
ADM guidance—Ceramics: Guidance to the use of fractography in failure analysis of brittle materials SS Scherrer, U Lohbauer, A Della Bona, A Vichi, MJ Tholey, JR Kelly, ... Dental materials 33 (6), 599-620, 2017 | 183 | 2017 |
Fractographic failure analysis of a Procera® AllCeram crown using stereo and scanning electron microscopy SS Scherrer, GD Quinn, JB Quinn Dental Materials 24 (8), 1107-1113, 2008 | 178 | 2008 |
Microstructural characterization and fracture behavior of a microhybrid and a nanofill composite SAR Junior, SS Scherrer, JL Ferracane, A Della Bona Dental materials 24 (9), 1281-1288, 2008 | 177 | 2008 |
Fracture toughness (KIc) of a dental porcelain determined by fractographic analysis SS Scherrer, JR Kelly, GD Quinn, K Xu Dental Materials 15 (5), 342-348, 1999 | 177 | 1999 |
Fractographic ceramic failure analysis using the replica technique SS Scherrer, JB Quinn, GD Quinn, HWA Wiskott Dental materials 23 (11), 1397-1404, 2007 | 176 | 2007 |
Failure analysis of ceramic clinical cases using qualitative fractography. SS Scherrer, JB Quinn, GD Quinn, JR Kelly International Journal of Prosthodontics 19 (2), 2006 | 175 | 2006 |
ADM guidance-ceramics: Fatigue principles and testing JR Kelly, PF Cesar, SS Scherrer, A Della Bona, R Van Noort, M Tholey, ... Dental Materials 33 (11), 1192-1204, 2017 | 155 | 2017 |
A nonlinear elastic model of the periodontal ligament and its numerical calibration for the study of tooth mobility G Pietrzak, A Curnier, J Botsis, S Scherrer, A Wiskott, U Belser Computer Methods in Biomechanics & Biomedical Engineering 5 (2), 91-100, 2002 | 145 | 2002 |
A new testing protocol for zirconia dental implants C Sanon, J Chevalier, T Douillard, M Cattani-Lorente, SS Scherrer, ... Dental Materials 31 (1), 15-25, 2015 | 143 | 2015 |
Grinding damage assessment for CAD-CAM restorative materials P Curran, M Cattani-Lorente, HWA Wiskott, S Durual, SS Scherrer Dental Materials 33 (3), 294-308, 2017 | 126 | 2017 |